Green concrete is mainly to protect
environmental pollution and for sustainable
development. It mainly consists of recycled concrete
aggregate, waste building concrete, etc. The properties
of natural aggregate is differ from the recycled coarse
aggregate. The properties of hardened concrete are
compared with different water-cement ratio. The
hardened concrete is observed using washed recycled
coarse aggregate. Recycled aggregate is generally used
to increase the creep and drying shrinkage. It decreases
the modulus of elasticity and compressive strength when
compared to natural aggregate. The recron 3S polyester
fibre is added to give additional strength to the
concrete. This fibre is added as 0.5%, 1%, and 1.5% by
volume of cement in order to improve its performance
and to reduce cracks. The test conducted for M30 grade
concrete is compressive strength, split tensile strength
and flexural strength. It is cured and tested after 7
days, 14 days, and 28 days and the optimum dosage of
recron 3S is compared.
Keywords : Recycled Concrete Aggregate, Recycled Aggregate, Recron 3S Polyester Fibre.